Scientists from Yokohama National University and Shimane University in Japan jointly with their colleagues from the National Synchrotron Radiation Research Center in Taiwan (China) have found a way to slow down capacity loss in lithium batteries with nickel-based cathodes. They achieved this by simply changing the composition of the liquid inside the battery, namely, by increasing the lithium salt content. At salt concentrations exceeding 3.5 mol/L, the cathode under study showed almost no capacity loss during tests.
Nickel is widely used in the cathodes of modern lithium-ion batteries. Increasing its proportion helps improve the battery’s energy density while also reducing or completely eliminating the need for cobalt. However, there is a downside to this solution: during charging, the surface of the nickel cathode becomes less stable and interacts more actively with the electrolyte. This causes undesirable chemical reactions that eventually lead to a decline in battery capacity.
The electrolyte is the liquid inside the battery that allows lithium ions to move between the electrodes. Generally, the lithium salt concentration in the electrolyte stands at about 1 mol/L. The researchers decided to look into what would happen if its concentration were increased. In their experiments, they used a cobalt-free lithium-nickel cathode and electrolytes with salt concentrations ranging from 1 mol/L to 5 mol/L.
At low salt concentrations, a large number of free solvent molecules remain in the electrolyte. At high voltages, these molecules engage in undesirable reactions with the surface of the nickel cathode, causing it to gradually lose its properties. However, the situation changes when the salt concentration reaches about 3.5 mol/L: nearly all solvent molecules become bound to lithium ions and can no longer interact as actively with the cathode. As a result, the number of undesirable reactions is significantly reduced, with capacity loss virtually ceasing.
Tests have confirmed this effect. At a salt concentration of 1 mol/L, the cathode capacity gradually declined with each charge-discharge cycle. As the salt content increased, these losses went down, virtually ceasing at concentrations above 3.5 mol/L. The scientists also observed a sharp reduction in the production of CO₂, a byproduct of undesirable reactions between the solvent and the cathode at high voltages.
However, the salt content cannot be increased indefinitely. The higher the concentration, the more viscous the electrolyte becomes, making it more difficult for lithium ions to move within the battery. For instance, ionic conductivity was roughly five times lower at a concentration of 5 mol/L than at 1 mol/L. If the electrolyte is too viscous, it also penetrates the electrodes less effectively.
This is why a concentration of 4 mol/L proved optimal in the experiments. At this concentration, the electrolyte essentially prevented capacity loss while still conducting lithium ions better than a more concentrated solution. These results could help develop high-energy lithium batteries with cobalt-free nickel cathodes. At the same time, reduction of the viscosity of concentrated electrolytes remains a key challenge for the future.